Baker Hughes has pioneered a solution to overcome flexible pipe stress corrosion cracking (SCC) tendencies in high CO2 content fields, such as those found in Brazil’s pre-salt offshore developments, the company said on March 22.
The inspection, verification and assurance body, Lloyd’s Register, issued Baker Hughes a design appraisal document (DAD) certification, validating the company’s flexible pipe testing program and results. This follows an extensive three-year testing campaign by Baker Hughes—featuring more than 120 test setups, methodologies and characterizations, including dissection of pipes recovered from field operations—and marks a step towards a viable flexible pipe solution for the most demanding high CO2 offshore fields. The certification verifies that on top of the standard 25- to 30-year equipment service life, Baker Hughes can extend flexible pipes contracted service life by at least 50%, with the potential of 2.5x life extension.
In 2017, the Brazil National Petroleum Agency issued a failure mode alert when it first identified flexible pipes used in high-pressure, high-CO2 content fields caused broken tensile armor wires on a flexible pipe installation with potential environmental impacts and production losses. The DAD offers a path forward for the growth of flexible pipes to meet the safety and regulatory requirements in the oil and gas industry.
“As an energy industry, we must constantly share lessons learned to ensure safe, reliable and environmentally sound operations. Baker Hughes applied its technology expertise to pioneer a solution to solve this challenge,” Domenico Di Giambattista, vice president for flexible pipe systems at Baker Hughes, said. “While the SCC-CO2 phenomenon was not something we experienced with our flexible pipes, it threatened the viability of certain offshore fields that require flexible pipe for development. This certification is an important step as we invest for growth to fully deploy flexible pipe systems in tough offshore environments.”
The DAD confirms that the combination of advanced materials and state-of-the-art manufacturing processes produces a flexible pipe that can withstand the most severe operating conditions while still retaining advantages including flexibility in field layout, simplified FPSO balcony configuration, and reduced time to first oil. Moving forward, all installed flexible pipes by Baker Hughes in Brazil will be covered by the DAD and offer operators extended operating life before replacement. In addition, the DAD enables Baker Hughes to assess and predict the integrity of flexible pipes operating for several years.
Baker Hughes is committed to future flexible pipe testing to further advance its unique technology.
Recommended Reading
Kissler: Gas Producers Should Still Hedge on Price
2025-03-27 - Recent price jumps and rising demand don’t negate the need to protect against future drops.
Plains All American President Pefanis to Retire
2025-03-27 - Current CEO Willie Chiang will take over as the next president of Plains All American Pipeline following co-founder Harry Pefanis’ retirement.
Japan’s JAPEX Backs Former TreadStone Execs’ New E&P Peoria
2025-03-26 - Japanese firm JAPEX U.S. Corp. made an equity investment in Peoria Resources, led by former executives from TreadStone Energy Partners.
CPP Wants to Invest Another $12.5B into Oil, Gas
2025-03-26 - The Canada Pension Plan’s CPP Investments is looking for more oil and gas stories—in addition to renewable and other energies.
Shell Raises Shareholder Distributions and LNG Sales Target, Trims Spending
2025-03-25 - Shell trimmed its annual investment budget to a $20 billion to $22 billion range through 2028 after spending $21.1 billion last year.